Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.7040 GPa | 102.1 ksi | 2% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |