Polymer Property : Flexural Modulus = 0.9653 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.9653 GPa
140.0 ksi
2% Secant; ASTM D790
ExxonMobil HD 6605.70 Injection Molding Resin
Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan..
Flexural Modulus 0.9653 GPa
140.0 ksi
2% Secant; ASTM D790
ExxonMobil HD 6733.17 Injection Molding Resin
Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable ..