Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.06 GPa
154 ksi
Chord; 2 mm/min; ISO 178
Mytex Polymers AS78L-GM Polypropylene, Rubber modified, Compounded
Description: AS78L-GM is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key..
Flexural Modulus 1.06 GPa
154 ksi
Dow DOWLEX™ IP-41 High Density Polyethylene
DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo..