Material Notes:
Description: AS78L-GM is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key Applications: Bumper fascias, cladding and bodyside moldingInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Ash 7.0 %
7.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ISO 868
Tensile Strength, Yield 16.0 MPa
2320 psi
50 mm/min; ISO 527
Flexural Modulus 1.06 GPa
154 ksi
Chord; 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 50.0 kJ/m²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-1