Polymer Property : Flexural Modulus = 1.135 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene
Copolymer Polypropylene, Unreinforced, 30 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, ..
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene
DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman.
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene
DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman.