Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.266 GPa
183.6 ksi
ASTM D790
Braskem BT 100K HDPE Blow Molding Polyethylene  (discontinued **)
Applications: Large containers from 60 to 200 litersInformation provided by Braskem
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.
Flexural Modulus 1.266 GPa
183.6 ksi
at 1.3 mm/min; ASTM D790
A. Schulman POLYFORT™ PP 3726
Information provided by A. Schulman.