Braskem BT 100K HDPE Blow Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem BT 100K HDPE Blow Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Large containers from 60 to 200 litersInformation provided by Braskem
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 144 hour

@Thickness 3.00 mm,
Temperature 23.0 °C
144 hour

@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693B
High Load Melt Index 7.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Flexural Modulus 1.266 GPa
183.6 ksi
ASTM D790
Izod Impact, Notched 6.70 J/cm
12.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Users viewing this material also viewed the following: