Mechanical Properties Metric English Comments
Flexural Modulus 0.00900 GPa
1.31 ksi
1% Secant
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber  (discontinued **)
A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica..
Flexural Modulus 0.00900 - 0.130 GPa
1.31 - 18.9 ksi
Average value: 0.0566 GPa Grade Count:17
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 0.00900 GPa
1.31 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-781 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs..
Flexural Modulus 0.00900 GPa
1.31 ksi
ASTM D638
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate
LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula..
Flexural Modulus 0.00900 GPa
1.31 ksi
ASTM D638
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride