Mechanical Properties Metric English Comments
Flexural Modulus 0.0100 GPa
1.45 ksi
ISO 178
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion
Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree..
Flexural Modulus 0.0100 - 51.7 GPa
1.45 - 7500 ksi
Average value: 5.34 GPa Grade Count:212
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Flexural Modulus 0.0100 GPa
1.45 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East)
Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 0.0100 GPa

@Temperature 49.0 °C
1.45 ksi

@Temperature 120 °F
ASTM D790
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.0100 GPa
1.45 ksi
ASTM D638
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme..