Mechanical Properties Metric English Comments
Flexural Modulus 0.0100 - 51.7 GPa
1.45 - 7500 ksi
Average value: 5.34 GPa Grade Count:212
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..