Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.96 - 10.1 GPa | 284 - 1460 ksi | Average value: 4.85 GPa Grade Count:43 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |