Flexural Modulus 10.16 GPa
1474 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT
LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 10.16 GPa
1474 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific)
LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 10.16 GPa
1474 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp AF008 ABS
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 10.16 GPa
1474 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp AF008 ABS (Asia Pacific)
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 10.16 GPa
1474 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer
LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled.
Flexural Modulus 10.16 GPa
1474 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.