Polymer Property : Flexural Modulus = 10.29 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.29 GPa
1492 ksi
ASTM D790
SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific)
40% GF/MF filled FR PPE/PS blend, high flow
Flexural Modulus 10.29 GPa
1492 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON PX91200 PA 6
LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural