Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.29 GPa | 1492 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific) 40% GF/MF filled FR PPE/PS blend, high flow |
|||
Flexural Modulus | 10.29 GPa | 1492 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON PX91200 PA 6 LNP VERTON* PX91200 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added features of this material include: High Impact, Structural |