Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.412 GPa | 1075 ksi | ASTM D790 |
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |