Mechanical Properties Metric English Comments
Flexural Modulus 11.39 GPa
1652 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 11.39 GPa
1652 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 11.39 GPa
1652 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 11.39 GPa
1652 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.