Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.39 GPa | 1652 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 11.39 GPa | 1652 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 11.39 GPa | 1652 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 11.39 GPa | 1652 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |