Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 (Asia Pacific) LNP* Verton* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |