Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.9 GPa @Thickness 6.40 mm |
1880 ksi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Flexural Modulus | 12.9 GPa @Thickness 6.40 mm |
1880 ksi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Flexural Modulus | 13.0 GPa | 1880 ksi | LW; ASTM D790 |
Haysite H1000 Polyester Laminate Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide.. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33E PEEK LNP LUBRICOMP* LCL33E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Easy Molding, Wear Resistant. |
|||
Flexural Modulus | 13.0 GPa | 1880 ksi | |
BCC Products BC 5010 Epoxy Laminating System BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor.. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 LNP VERTON* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 12.96 GPa | 1880 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Verton PV00A PA 6 (Asia Pacific) LNP* Verton* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |