Polymer Property : Flexural Modulus = 1271 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 8.763 GPa
1271 ksi
ASTM D790
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.