Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.890 GPa @Temperature 60.0 °C |
129 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 0.892 GPa | 129 ksi | ASTM D790 |
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin
(discontinued **) MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | |
Kraton® G1652 + PP blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ASTM D790 |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.889 GPa | 129 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.889 GPa | 129 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100L (COND, 50% RH) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.889 GPa | 129 ksi | |
Dow HDPE 04452N High Density Polyethylene DOW HDPE 04452N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and stacking strength with excellent impact strength. This resin has moderate.. |
|||
Flexural Modulus | 0.889 GPa | 129 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Conditioned Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |