Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.7 GPa | 1990 ksi | ASTM D790 |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | ASTM D790 |
Kolon KOCETAL® CF704 Conductive Grade Acetal Resin Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Flexural Modulus | 13.7 GPa @Thickness 6.40 mm |
1990 ksi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Flexural Modulus | 13.7 GPa @Thickness 3.20 mm |
1990 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 13.7 GPa @Thickness 3.20 mm |
1990 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Flexural Modulus | 13.7 GPa | 1980 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance.. |
|||
Flexural Modulus | 13.7 GPa | 1980 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta.. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | ASMT D790 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Flexural Modulus | 13.7 GPa | 1990 ksi | ASTM D790 |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |