Flexural Modulus 13.7 GPa
1980 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance..
Flexural Modulus 13.7 GPa
1980 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta..