Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.9 GPa @Temperature 23.0 °C |
2020 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ISO 178 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC004XXP PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC004XXP is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features include; Electrically Conductive. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ASTM D790 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ASTM-D790 |
Polyram Polytron P60B01 Homopolymer Polypropylene, Chemically Coupled 60% LGF A chemically coupled 60% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | ASTM-D790 |
Polyram Polytron P60B11 Homopolymer Polypropylene, Chemically Coupled 60% LGF A chemically coupled 60% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 13.9 GPa | 2020 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |