Mechanical Properties Metric English Comments
Flexural Modulus 9.86 - 9.86 GPa

@Temperature 232 - 232 °C
1430 - 1430 ksi

@Temperature 450 - 450 °F
Average value: 9.86 GPa Grade Count:1
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..