Mechanical Properties Metric English Comments
Flexural Modulus 0.992845 - 5.19865 GPa

@Temperature -40.0 - 121 °C
144.002 - 754.012 ksi

@Temperature -40.0 - 250 °F
Average value: 2.30 GPa Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..