Mechanical Properties Metric English Comments
Flexural Modulus 10.76 GPa
1561 ksi
ASTM D790
Plenco 50130 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..