Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.94 GPa | 1587 ksi | ASTM D790 |
Plenco 50130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |