Polymer Property : Flexural Modulus = 16.78 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 16.78 GPa
2434 ksi
ISO 178
Solvay TECHNYL® A 118L V50 PA66, 50% glass fiber, Eh 0
Description: TECHNYL A 118L V50 is a polyamide 6.6 reinforced with 50% of glass fiber, with thermal stability, UV protection and modified viscosity that provides better superficial appearance. Color..