Mechanical Properties Metric English Comments
Flexural Modulus 1.210 GPa
175.5 ksi
ASTM D 790
Total 50100.2 HDPE blow molding, sheet, thermoforming resin
Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging, sheet extrusion, thermoforming, truck bed liners, dunnage containers..