Polymer Property : Flexural Modulus = 1760 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.1 GPa
1760 ksi
ASTM D790
Techmer ES Plastiblend® PBT/ABS GF/M40 FR 40/40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Fiber Reinforcement, 40/40% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Flexural Modulus 12.1 GPa
1760 ksi
ASTM D-790
Glastic GLASGUARD Scuff and Bulkhead Liners
GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib..