Flexural Modulus 12.84 GPa
1862 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific)
LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s).
Flexural Modulus 12.84 GPa
1862 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA
LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s).