Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0139 GPa | 2.02 ksi | ASTM D790 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |
|||
Flexural Modulus | 0.0139 GPa | 2.02 ksi | 1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790 |
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low .. |