Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.158 GPa | 313.0 ksi | ASTM D790 |
Kolon KOCETAL® LF302 Wear Modified Acetal Resin Improved wear property and dimensional stability. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.158 GPa | 313.0 ksi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid prod.. |