Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.42 GPa
351 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.42 GPa
351 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycolac® FR30U ABS
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.42 GPa
351 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific)
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.
Flexural Modulus 2.42 GPa
351 ksi
1.3 mm/min; ASTM D790
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified
Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi..
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer
LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant.
Flexural Modulus 2.42 GPa
351 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Flexural Modulus 2.42 GPa
351 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Flexural Modulus 2.42 GPa
351 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.42 GPa
351 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.42 GPa
351 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
Flexural Modulus 2.42 GPa
351 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
Flexural Modulus 2.42 GPa
351 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer
LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
Flexural Modulus 2.42 GPa
351 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
Flexural Modulus 2.42 GPa
351 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific)
High heat PPO/HIPS alloy suitable for use in some potable water applications.
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Flexural Modulus 2.42 GPa
351 ksi
2mm/min; ASTM D790
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Flexural Modulus 2.42 GPa
351 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..