Polymer Property : Flexural Modulus = 2.423 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.423 GPa
351.4 ksi
ASTM D790M
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..