Mechanical Properties Metric English Comments
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS
PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12
LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1020 PP
SABIC® PPcompound 19T1020 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application..
Flexural Modulus 2.49 GPa
361 ksi
0.125 in, injection molded, unannealed; ASTM D790
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Flexural Modulus 2.49 GPa
361 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL N225X PPE+PS
PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications.
Flexural Modulus 2.49 GPa
361 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Flexural Modulus 2.49 GPa
361 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating ..
Flexural Modulus 2.49 GPa
361 ksi
ISO 178
Polyplastics Duranex® 407EP Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 2.49 GPa
361 ksi
ASTM D790
CPC - Vycom Corzan® CPVC Chlorinated PVC
Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup..
Flexural Modulus 2.49 GPa
361 ksi
JIS-K-6740
Denka VINYKON R3105 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Flexural Modulus 2.49 GPa
361 ksi
ASTM D-790
Axiall 7768 Rigid PVC, Extrusion
Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..