Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.507 GPa | 363.6 ksi | ASTM D790 |
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren.. |