Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC (Asia Pacific) ASA+PC blend. Weatherable, injection grade. Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ISO data |
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8200 HS BK-102 is a medium viscosity, heat stabilized, pigmented black, nylon 6 injection molding homopolymer exhibiting resistance to sink-mark formation in thick section, and improved tough.. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | Molded; ASTM D790 |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific) |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl 534 PPE+PS High heat, unreinforced.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | ASTM D-790 |
Axiall 3152 Rigid PVC, Extrusion Georgia Gulf 3152 is a twin screw powder blend NSF approved for the extrusion of potable water and drain waste and vent pipe application.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Flexural Modulus | 2.58 GPa | 374 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |