PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Density 0.801 g/cc
0.0289 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Hardness, Shore D 79
79
ASTM D2240
Tensile Strength, Yield 43.4 MPa
6290 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.39 GPa
347 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.58 GPa
374 ksi
ASTM D790
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 59.4 °C

@Thickness 3.18 mm
139 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 81 %

@Thickness 0.851 mm,
Wavelength 400 nm
81 %

@Thickness 0.0335 in,
Wavelength 400 nm
Internal Method
86.5 %

@Thickness 0.851 mm,
Wavelength 700 nm
86.5 %

@Thickness 0.0335 in,
Wavelength 700 nm
Internal Method
Processing Properties Metric English Comments
Mold Temperature 202 - 213 °C
396 - 415 °F
Blow Molding
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
High Gloss
High Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Bottles
Packaging