Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS) Information provided by PolyOne |
|||
Flexural Modulus | 20.0 - 22.0 GPa | 2900 - 3190 ksi | ISO 178 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Flexural Modulus | 20.0 GPa @Temperature 23.0 °C |
2900 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1105-8496 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 20-7970 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 865M Novolac Phenolic Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |