Mechanical Properties Metric English Comments
Flexural Modulus 6.00 - 21.0 GPa
870 - 3050 ksi
Average value: 9.46 GPa Grade Count:32
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Flexural Modulus 8.60 - 21.0 GPa
1250 - 3050 ksi
Average value: 15.1 GPa Grade Count:51
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Flexural Modulus 3.10 - 21.0 GPa
450 - 3050 ksi
Average value: 9.79 GPa Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..