Flexural Modulus 1.517 GPa
220.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 3012 Natural 30% Calcium Carbonate Polypropylene
This material is an impact modified Calcium Carbonate filled polypropylene that has good impact resistance, good basic UV resistance, and is easily colored. UV additives can be used for extended UV..
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers
High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat..
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Total PPH 3860X Polypropylene, Extrusion Grade
High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA..
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Eastman Tenite 350A0096914 Propionate Natural
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Diamond Polymers NPP25-1201 TF10 10% Talc Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..