Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 3012 Natural 30% Calcium Carbonate Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is an impact modified Calcium Carbonate filled polypropylene that has good impact resistance, good basic UV resistance, and is easily colored. UV additives can be used for extended UV protection.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955-89
Melt Flow 12 g/10 min
12 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638-95
Elongation at Break 165 %
165 %
ASTM D638-95
Flexural Strength 29.3 MPa
4250 psi
ASTM D790-95
Flexural Modulus 1.517 GPa
220.0 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256-93a
Gardner Impact 23.7 J
17.5 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648-95