Mechanical Properties Metric English Comments
Flexural Modulus 152 GPa
22000 ksi
Typical epoxy composite property
Hexcel® HexTow™ IM9 Carbon Fiber
HexTow™ IM9 carbon fiber is a continuous, ultrahigh performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be s..