Mechanical Properties Metric English Comments
Flexural Modulus 15.61 GPa
2264 ksi
ASTM D790
SABIC Innovative Plastics LNP KONDUIT OTF2B PPS - Linear
LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.