Polymer Property : Flexural Modulus = 233 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.61 GPa
233 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S950
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.