Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 17.9 GPa @Temperature 23.9 °C |
2600 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF33 ML2 BK 33% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceAp.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Ecomass® 1850ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)RigidInformation provided by Technical Polymers |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Ensinger Tecapeek® XP-111 Compression Molded PEEK Compound, 50% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Modulus | 17.9 GPa | 2600 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |