Mechanical Properties Metric English Comments
Flexural Modulus 1.83 GPa
265 ksi
Tangent; ASTM D790
RheTech Products GC10P200-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural
Applications: Component housingsStorage binsRecreational vehicle trim and bumpersInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.83 GPa
265 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 30-2000 NA
Description: Homopolymer Polypropylene Nucleated with AntistatInformation provided by Network Polymers Inc.
Flexural Modulus 1.83 GPa
265 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
Flexural Modulus 1.83 GPa

@Thickness 3.17 mm
265 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-3013 High Flow PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Flexural Modulus 1.83 GPa
265 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® ML6018R PC (Asia Pacific)
ML6018R is a low viscosity grade exhibiting a high impact performance over standard PC. It contains an enhanced release-agent. Opaque colours only.This data was supplied by SABIC-IP for the Asia Pac..
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790A
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject..
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074..
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790B
Ineos N01N-00 Polypropylene Impact Copolymer
Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti..
Flexural Modulus 1.83 GPa
265 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL SPN410 PPE+PS
Improved productivity. 210F (99C) DTUL. UL94 HB rated.
Flexural Modulus 1.83 GPa
265 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific)
Designed for outdoor telecommunications enclosure applications.
Flexural Modulus 1.83 GPa
265 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.83 GPa
265 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA
Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications..
Flexural Modulus 1.83 GPa
265 ksi
Tangent; ASTM D790
Plastics Group Polifil® RMT-10 10% Talc-Reinforced Polypropylene, High Impact
Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P..
Flexural Modulus 1.83 GPa
265 ksi
ASTM D790
Multibase Multi-Flam™ 0102 PP Polypropylene
Features:Flame RetardantHalogenated Forms:PelletsProcessing Methods:Injection MoldingBlow MoldingExtrusionUses:TubingInformation provided by Multibase