Mechanical Properties Metric English Comments
Flexural Modulus 1.84 GPa
267 ksi
Tangent; ASTM D790
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..
Flexural Modulus 1.84 GPa
267 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Opnyl OP66UT108 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Flexural Modulus 1.84 GPa
267 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.84 GPa
267 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific)
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 1.84 GPa
267 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT
4.2 specific gravity, PBT, gray